MOLE FLEXIBLE

Corrosion

During reactor charging and centrifuge discharge, flexible connectors may contact powders containing strong acids, strong bases, polar solvents or nonpolar solvents. The sleeve material must withstand chemical exposure while remaining flexible.

Examples of process media

Acids

  • Sulfuric acid H₂SO₄
  • Nitric acid HNO₃
  • Hydrochloric acid HCl
  • Hydrobromic acid HBr
  • Hydroiodic acid HI
  • Perchloric acid HClO₄
  • Phosphoric acid H₃PO₄

Bases

  • Sodium hydroxide NaOH
  • Potassium hydroxide KOH
  • Lithium hydroxide LiOH
  • Calcium hydroxide Ca(OH)₂
  • Aqueous ammonia NH₃(aq)

Polar solvents

  • N-Methyl-2-pyrrolidone NMP
  • Dimethylformamide DMF
  • Dimethyl sulfoxide DMSO
  • Acetone (CH₃)₂CO
  • Acetonitrile CH₃CN
  • Tetrahydrofuran THF

Nonpolar and other solvents

  • n-Hexane C₆H₁₄
  • Cyclohexane C₆H₁₂
  • Toluene C₆H₅CH₃
  • Xylene C₆H₄(CH₃)₂
  • Petroleum ether
  • Dichloromethane CH₂Cl₂
  • Carbon tetrachloride CCl₄

Corrosion Cases

Toluene C₆H₅CH₃
Dichloromethane CH₂Cl₂
Thionyl chloride SOCl₂

TE02 / TE02AS

TE02 and TE02AS are flexible PTFE grades designed to resist attack from a wide range of chemicals. Confirm compatibility of the complete connection for the actual chemical mixture, concentration, temperature and exposure time.

TE02
TE02AS